Weifang Duojiao Chemical Co.,Ltd

GOOD QUALITY, GOOD SERVICE, FAST DELIVERY.

Home
Products
About Us
Factory Tour
Quality Control
Contact Us
Request A Quote
Home ProductsMagnesium Chloride Compound

Weifang Duojiao Chemical Co.,ltd

Good quality Calcium Chloride Compound for sales
Good quality Calcium Chloride Compound for sales
My customers are satisfied with this product.

—— Mr. William

Good cacl2.

—— Kaled

I'm Online Chat Now

MgCl2 / Magnesium Chloride Snow Melting Agent For Airport , Stress Corrosion Resistance

China MgCl2 / Magnesium Chloride Snow Melting Agent For Airport , Stress Corrosion Resistance supplier
MgCl2 / Magnesium Chloride Snow Melting Agent For Airport , Stress Corrosion Resistance supplier MgCl2 / Magnesium Chloride Snow Melting Agent For Airport , Stress Corrosion Resistance supplier

Large Image :  MgCl2 / Magnesium Chloride Snow Melting Agent For Airport , Stress Corrosion Resistance

Product Details:

Place of Origin: Shandong,China
Brand Name: Haibin
Certification: ISO9001

Payment & Shipping Terms:

Minimum Order Quantity: 19tons
Price: Negotiable
Packaging Details: 25kg PP/PE bag or 500/1000kg Jumbo bag
Delivery Time: 7-15 days
Supply Ability: 1200tons per month
Contact Now
Detailed Product Description
Classification: Chloride Form: White / Light Yellow Flake
Aquatic Toxicity: Be In Accordance With The EPA / OECD. Boiling Point: 1412°C
PH Value: 8-10 Model Number: Melting-snow Agent

 

MgCl2 / Magnesium Chloride Snow Melting Agent For Airport , Stress Corrosion Resistance

 

Descriptions
 

  • Product Name: Magnesium Chloride / MgCl2
  • Appearance: Yellow / white flake
  • PH Value 8.0-10.0
  • Stress Corrosion Resistance: in accordance with ASTM F 945
  • Runway Concrete Scaling Resistance: in accordance with ASTM C 672. Performing more than one freeze-melting experiment , its damage to part even less than that of tap-water.
  • Plant Salt Resistance Test:It is good for the growth of plant without negative effect.
  • Aquatic Toxicity: It is in accordance with the EPA (40 Code of Federal Regulations (CFR) Parts 797.1300 and 797.1400) or OECD (Organization for Economic Cooperation and Development Guidelines for Testing of Chemicals , Method 202 and 203) .
  • Pollution: Pollution It is in accordance with the regulations of (Standard Method for Examination of Water and Wastewater) from USA.

 

Product Details

 

Product Name Magnesium Chloride / MgCl2
Purity 98%min
Molecular Weight 95.2
Color Pure White , Yellow
Melting Point 714°C
Boiling Point 1412°C
Grade Industrial Grade , Medecine Grade , Argiculture Grade
Applications Manufacturing of alloys
Grain refining of metal
Texile 

 

SPECIFICATIONS RESULTS
MgCl2 46%min
K 0.0001%
Na 0.0002%
S 0.0003%
Fe 0.0001%
Ca 0.14%max
PH 7-9
Water Insoluble 0.12%max

 

Applications

 

  • As snow - melting agent.
  • Snow - melting agent for Airport is researched and developed as a new kind of environment - friendly snow - melting agent for melting the ice and snow in airstrip , parking apron and taxiway in very short time.
  • Compared with the traditional melting method in blow way , it can save energy and time.

 

Packing&Shipping

 

  • Package

    Plastic woven bag with PE liner.

  • Packing

    25kg PP / PE bag or 500 / 1000kg Jumbo bag or as customer's demand.
    25 - 26mt in 1*20fcl without pallet ,19mt in 1*20fcl with pallet.

  • MOQ 19tons

 

Our services

 

1. Focusing on MgCl2 , we now boast customers in more than 30 countries.

2. The most suitable package which can protect the MgCl2 well.

3. Timely delivery.

4. We have own warehouse and select high quality to export.

5.  Timely and reasonable claims , if something has gone wrong in our products , we will send you ten times replacement ASAP.

 

MgCl2 / Magnesium Chloride Snow Melting Agent For Airport , Stress Corrosion Resistance

 

Contact Details
Weifang Duojiao Chemical Co.,ltd

Contact Person: april

Send your inquiry directly to us (0 / 3000)